Shanghai Tankii Alloy Material Co.,Ltd

Shanghai Tankii Alloy Material Co.,Ltd First Quality, Sincere Service

Manufacturer from China
Verified Supplier
11 Years
Home / Products / Precision Alloy /

Dia. 0.05mm Precision Alloy Iron Nickel Alloy Wire Permalloy 1j50/ Ni50 / E11a / FeNi50 / 50H

Contact Now
Shanghai Tankii Alloy Material Co.,Ltd
Visit Website
City:shanghai
Province/State:shanghai
Country/Region:china
Contact Person:MrMartin Lee
Contact Now

Dia. 0.05mm Precision Alloy Iron Nickel Alloy Wire Permalloy 1j50/ Ni50 / E11a / FeNi50 / 50H

Ask Latest Price
Video Channel
Brand Name :TANKII
Model Number :FeNi50
Certification :ISO SGS
Place of Origin :Shanghai, China,
MOQ :Negotiable
Price :negotiable
Payment Terms :L/C, T/T, Western Union
Supply Ability :100 Tons per Month
Delivery Time :7-15 work days
Packaging Details :wooden case
Material :Iron Nickel Alloy
Dia. :0.02mm
Surface :Bright / Polished
Sample :accepted
Shape :Pipe/wire/rod/strip/plate/coil
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Permalloy 1j50/ Ni50 / E11a Wire Precision Alloy FeNi50 50H
Brand: 1J50

Classification: Alloys of precision soft magnetic
Supplement: alloy has a high permeability and low saturation induction of technical
Application: For cores between the tube and small power transformers, chokes, relays and parts of magnetic circuits operating at elevated inductions without bias or small bias

Chemical Composition in % 1J50


Ni
49-50.5%

Fe
48.33-50.55%

C
0.03%

Si
0.15 - 0.3%

Mn
0.3 - 0.6%

S
o 0.02%

P
0.02%

Mo
-

Ti
-

Al
-

Cu
0.2%


Basic physical constants and mechanical properties of the alloy:

Density: γ = 8,2 g / cm3;
Electric resistivity: ρ = 0,45 ohm mm2 ? / m;
Curie Point Temperature: Θs = 500 ° C;
Saturation magnetostriction: λS = 25 ? 106;
Brinell Hardness: 170/130 HB;
Ultimate: Rm = 780/440 MPa;
Yield strength: σ0,2 = 685/145 MPa;
Modulus of elasticity E = 160 kN / mm2;
Elongation: δ5 = 3/35%;
Relative compression: φ = 15/60%.

The magnetic properties of the alloy

Type Class Thickness or diameter, mm The initial magnetic permeability Maximum magnetic
permeability
Coercive force Technical saturation induction
mH / m G / E mH / m G / E / E (10-4 G)
No more No more No less
cold-rolled strips 1 0,05
0,08

2,5

2000

25

20000

20

0,25
1,50
0,10
0,15

2,9

2300

31

25000

16

0,20
0,20
0,25
0,27

3,3

2600

38

30000

12

0,15
0,35
0,50

3,8

3000

44

35000

10

0,12
0,80
1,0

3,8

3000

38

30000

12

0,15
1,5
2,0
2,5

3,5

2800

31

25000

13

0,16
hot rolled sheets 3-22 3,1 2500 25 20000 24 0,30
Bars 8-100 3,1 2500 25 20000 24 0,30
cold-rolled strips 2 0,10
0,15

3,8

3000

38

30000

14

0,18
0,20
0,25

4,4

3500

44

35000

12

0,15
0,35
0,50

5,0

4000

56

45000

10

0,12
0,80
1,0

5,0

4000

50

40000

10

0,12
1,5
2,0

3,8

3000

44

35000

12

0,15
cold-rolled strips 3 0,05
0,10
0,20

12,5
*

10000
*

75

60000

4,0

0,05
1,52

2.Usage
It is mostly used in small transformers, pulse transformers, relays, transformer, magnetic amplifier, electromagnetic clutch,the reactor coreand magnetic shielding which work inweak magnetic orsecondary magnetic field.

3.Features
1).Low coercivity and magnetic hysteresis loss;
2).High resistivity and loweddy-currentloss;
3).High initialmagnetic permeability and maximum magnetic permeability;
4).High saturation magnetic flux density;

4. Packing detail
1). Coil (plastic spool) + compressed ply-wooden case + pallet
2). Coil (plastic spool) + carton + pallet
5. Products and services

Dia. 0.05mm Precision Alloy Iron Nickel Alloy Wire Permalloy 1j50/ Ni50 / E11a / FeNi50 / 50H

Inquiry Cart 0